Sc2O3values describe: Sc₂O₃-doped W
Vacuum electronics & X-ray sources
What it enables
Scandia-doped tungsten dispensers emit at lower temperature and higher density than B and M types: longer tubes, denser beams, the next rung of the cathode ladder.
Status and pusher
Reproducibility and life data still maturing; pushed by the vacuum electronics community (IVEC circuit) and mm-wave TWT programs.
Watch out
Emission uniformity is the historic failure mode.
Properties
The values below are candidate: compiled from the sources named, not yet individually validated.
Provisional provenance: Electron tube and ceramic-to-metal sealing practice.
Wet cleaning
| Recipe | never: the impregnant is water reactive |
|---|
| Forbidden | moisture and air exposure after activation |
|---|
| Limit | poisoning by oxygen and water, measured in ppm |
Vacuum and outgassing
| Vapour pressure | barium and scandium evaporate by design |
Temperature
| Vacuum degas | 1200 °C |
|---|
| Metallurgical limit | activation 1100–1200 °C |
Electrical and magnetic
| Relative permeability | ~1.0 |
Engineering
| Process notes | 10 A/cm² at lower temperature than any current cathode |
|---|
| Availability and cost | research and specialist tube makers |
Grades
| Scandia-doped W dispenser | lab and pilot tubes |
Sources · 1
- IVEC proceedings, scandate cathode sessions